As one of the key technologies in modern advanced manufacturing, laser welding is widely used in the automotive, electronics, aerospace, mechanical processing and other industries due to its fast welding speed, small heat-affected zone and beautiful weld. In practical applications, depending on the welding object, there are significant differences in the process of laser welding technology on thin and thick metal plates. This article will deeply explore the process differences between thin and thick laser welding from the aspects of energy control, process parameters, welding methods, common problems, etc.

Definition of thin and thick plates


Usually, metal plates with a thickness of less than 3mm are classified as “thin plates”, such as stainless steel housings and electronic parts; those with a thickness of more than 3mm are classified as “thick plates”, such as steel structural components and mold bases. The two types of materials have significant differences in requirements for laser energy input, penetration depth, penetration width, thermal management, etc. during welding.

Process characteristics of laser welding thin plates


1. Low energy and high precision control

Thin plate materials are easy to burn through, so the laser energy needs to be precisely controlled, and low-power lasers (such as 500W~1500W) are usually used.
The focus position requirements are very high, and a deviation of 1mm may cause welding through.

2. Narrow weld and small heat-affected zone

The weld width is usually between 0.1 and 1 mm, and the material deformation is small during welding.
High-precision welding can be achieved, suitable for electronic packaging, battery housing and other fields.

3. Strong high-speed welding capability

Since thin plates have fast heat conduction and shallow melting depth, higher welding speeds (even exceeding 10 m/min) can be used to improve efficiency.

4. Main welding mode

The melting depth is shallow, and the heat conduction welding mode (Heat Conduction Welding) is usually used to avoid the formation of deep melting holes.

Process characteristics of laser welding thick plates


1. High-power laser supports deep melting welding

Thick plates usually require more than 2 kW of power (sometimes even more than 10 kW) to achieve penetration welding.
Using the keyhole welding mode, the laser beam melts through the material to form a small hole and enhances the melting depth.

2. The heat input and deformation control need to be balanced

The heat input during laser welding of thick plates is high. If it is not properly controlled, problems such as thermal cracks, weld collapse, and welding deformation are prone to occur.
It is necessary to reduce stress concentration through multi-pass welding, preheating, post-heating, clamping and other means.

3. Multi-layer multi-pass welding

For thick plate materials over 10mm, multi-layer pass welding is often used to fill the weld to ensure welding strength.

4. Weld detection is more critical

Thick plates are mostly used for structural parts, requiring welds to have higher strength and reliability, so non-destructive testing such as ultrasonic and X-ray is often required.

Challenges and solutions in practical applications


  • Common problems in thin plate weldingProblems: welding through, spatter, edge melting

Solution: Use a larger spot, control the focus position above the surface, and reduce power density.

  • Common problems in thick plate welding

Problems: incomplete penetration, cracks, holes
Solution: Increase laser power, preheat treatment, optimize welding path, multi-layer multi-pass welding.

Conclusion


The difference between thin and thick plate metals in laser welding technology is not only reflected in the difference in welding parameters, but also in the different requirements for welding technology accuracy, energy control, and deformation control. If you want to know more, please contact us!