How to Avoid Porosity in Laser Aluminum Welder?

Laser Aluminum Welder

Table of Contents

Porosity is one of the most common welding defects during laser welding of aluminum and aluminum alloys, severely impacting weld tightness and mechanical properties. To effectively reduce porosity, multiple approaches can be considered, including pre-weld preparation, process parameter control, shielding gas selection, and process innovation.

Classification of Weld Porosity


One type of porosity is caused by the drastic drop in hydrogen solubility during cooling during laser welding of aluminum alloys. The hydrogen content of molten aluminum alloy is as high as 69 mL/100 g, but drops to 0.36 mL/100 g after solidification. This leads to supersaturated hydrogen precipitation and the formation of hydrogen pores. Furthermore, during welding, the oxide film on the aluminum alloy surface decomposes directly into hydrogen from the crystalline water, air, and moisture in the shielding gas. These hydrogen pores are unable to escape quickly during the rapid cooling process and remain in the weld.
Another type of porosity is caused by unstable keyhole collapse during laser welding, which prevents the liquid metal from filling the keyhole, resulting in a cavity. Excessive porosity reduces weld density, weakens the joint’s load-bearing capacity, and leads to reduced joint strength and ductility.

How to Avoid Porosity in Laser Aluminum Welder?


1. Pre-weld Surface Treatment to Suppress Weld Porosity

Pre-weld surface treatment is an effective method for controlling metallurgical porosity in aluminum alloy laser welding. Generally, surface treatment methods include physical, mechanical, and chemical cleaning.

After comparison, the optimal process is a combination of mechanical cleaning and chemical treatment (metal detergent cleaning – water washing – alkaline washing – water washing – pickling – water washing – drying). Use a 25% NaOH aqueous solution to remove the surface thickness of the material during alkaline washing, and a 20% HNO3 + 2% HF aqueous solution to neutralize the residual alkaline during pickling. Remove oxide films and oil stains from the base metal and welding wire surfaces.

After surface treatment, test panels should be welded within 24 hours. If the test panels are left for an extended period after treatment, wipe the assembly with anhydrous alcohol before welding.

2. Controlling Weld Porosity with Welding Process Parameters

The formation of weld porosity is not only related to the surface finish quality of the weldment, but also to the welding process parameters. The impact of welding parameters on weld porosity is primarily reflected in weld penetration, specifically the effect of the weld back-to-width ratio on weld porosity.
The results show that a back-to-width ratio r > 0.6 effectively improves the concentration distribution of chain pores in the weld; a back-to-width ratio r > 0.8 effectively reduces the presence of large pores in the weld, largely eliminating any residual pores.

3. Controlling Weld Porosity by Selecting the Appropriate Shielding Gas and Flow Rate

Adding a small amount of CO2 or O2 to inert welding shielding gases such as Ar and He can help reduce porosity.
Recommendations:

  • Use high-purity argon or helium as the primary shielding gas;
  • Maintain a stable gas flow rate to avoid excessive gas flow that disrupts the weld pool;
  • Adjust the nozzle angle to ensure uniform gas flow coverage of the weld area.

Summary


Avoiding porosity in laser aluminum welder requires a systematic coordination of pre-weld cleaning, parameter optimization, gas control, and process innovation. Only by rigorously controlling each step can high-quality welds with a dense structure, excellent appearance, and stable performance be achieved.